Nylon 6 30% Glass Filled Technical Data
Property |
Test Method
|
Units
|
UNIPA MRg
|
|
|
|
30% Glass
Fiber Filled Nylon 6
|
Mechanical
|
Specific Gravity |
ASTM-D792
|
---
|
1.28
|
Tensile Strength |
ASTM-D638
|
psi
|
18,000
|
Tensile Elongation |
ASTM-D638
|
%
|
8
|
Tensile Modulus of Elasticity |
ASTM-D638
|
psi
|
|
Flexural Strength |
ASTM-D790
|
psi
|
25,000
|
Flexural Modulus of Elasticity |
ASTM-D790
|
psi
|
|
Compressive Strength |
ASTM-D695
|
psi
|
25,000
|
Izod Notched Impact |
ASTM-D256
|
ft.-lb./in.
|
1.0
|
Rockwell Hardness |
ASTM-D785
|
M or R
scale
|
M100
|
Thermal |
Coef. of Linear Thermal Expansion |
ASTM-D696
|
in./in./deg F
|
1.5 x 10-5 |
Max. Continuous Use Temp. |
Nytef
std.
|
°F
|
210
|
Heat
Deflection Temp. @ 264 psi
|
ASTM-D648
|
°F
|
300
|
Melting Point |
ASTM-D3418
|
°F
|
430
|
Electrical |
Dielectric Strength-Short Term |
ASTM-D149
|
volts/mil
|
500
|
Dielectric Constant @ 106 Hz |
ASTM-D150
|
|
3.7
|
Dissipation Factor @ 60 Hz |
ASTM-D150
|
|
.02
|
Volume Resistivity |
ASTM-D257
|
ohm-cm
|
>1013
|
Miscellaneous |
Water Absorption/24 hrs. |
ASTM-D570
|
% weight
|
0.4
|
Water Absorption @ Saturation |
ASTM-D570
|
% weight
|
3.5
|
Flammability |
UL-94
|
|
HB
|
Dynamic
Coefficient of Friction
|
|
|
0.33
|
Agency Approvals |
FDA/USDA |
|
|
No
|
3-A Dairy |
|
|
No
|
|
|