Conductive Isomolded Graphite Rods, Super Fine Grain | ||||
|
||||
PROPERTY | US VALUE | METRIC VALUE | ||
Density | 0.065 | lb/in 3 | 1.81 | gr/cm 3 |
Shore Hardness | 76 | |||
Flexural Strength | 7250 | psi | 50 | mpa |
Oxidizing Atmosphere | 801 | °F | 427 | °C |
Neutral Atmosphere | 5000 | °F | 2760 | °C |
Porosity | 12 | % | % | |
Electrical Resistivity | 0.00055 | ohm-inch | ohm-cm | |
Thermal Conductivity | 49 | BTU/(h.ft 2 °F/ft) | 85 | W/(m 2 . K/m) |
Ash Content | 100 | ppm | ||
CTE | 2.6 | in/in °F x 10 -6 | 4.6 | Microns/m °C |